Jamb & Exterior Coatings Binder

PHYSICAL PROPERTIES
Product NameChemical
Composition
Total Solids
(+/-1)
pH
Value
Viscosity
(Cps)
Tg *
(°C)
MFFT*
(°C)
Applications
KEMILINE CE 911S/AC576,0 - 9,0MAX. 6000-23<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 101S/AC507,0 - 9,0MAX. 800-22<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 930S/AC576,5 - 9,0150 - 1000-10<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 910S/AC576,0 - 9,0150 - 1200-6<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE RC 865S/AC507,0 - 9,01000 - 3000-6-1Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 903S/AC507,0 - 9,02000 - 8000-6<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 756S/AC506,0 - 9,05000 - 15000-3<0Roof coatings, Jamb
KEMILINE CE 757S/AC507,0 - 9,02000 - 8000-2< 0Roof coatings, Jamb
KEMILINE CE 808S/AC507,0 - 9,05000 - 160002222Jamb
KEMILINE CE 701AC479,0 - 10,0MAX. 4001510Crack fillers, Elastic coatings,
Moisture barriers
KEMILINE CE 902S/AC537,0 - 9,0MAX. 1500-35<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 917S/AC556,0 - 9,0MAX. 1000-6<0Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 900S/AC507,0 - 9,0MAX. 400010<3Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 117AC507,0 - 9,0MAX. 7000<3Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CB 560AC607,0 - 9,5MAX. 700083Roof coatings, Crack fillers,
Moisture barriers
KEMILINE CE 704AC506,0 - 9,0MAX. 600109Roof coatings, Crack fillers,
Moisture barriers


İtalic characters coded products are under development
(*): These are typical properties of the emulsions and should not be considered as specifications. Certificates of the analysis (COA) are available upon request.
AC: Pure Acrylic CopolymersVA/AC: Vinyl Acrylic CopolymersViscosity: Brookfield viscosity, mPa.s
S/AC: Styrene Acrylic CopolymersVA/Veova: Vinyl Acetate / Veova CopolymersTg (°C): Glass transition temperature
PVA: Poly Vinyl Acetate PolymersVV/AC: Vinyl Versatate / Acrylic therpolymerMFFT (°C): Minimum film formation temperature